Nickel-basesuperalloy相关论文
Thermo-mechanical fatigue behavior of nickel-base powder metallurgy superalloy FGH96 under tension-t
...
Anti-penetration characteristics of Nickel-base superalloy Inconel-718 under different impact veloci
In the present study, the ballistic impact tests of different target thickness (2mm, 3mm, 5mm and 6mm) and at differ......